Customer in Bengal ordered 4*20GP containers refractory fire bricks and ceramic fiber blankets
In January. 4*20 GP containers refractory fire bricks and ceramic fiber blankets are packed for delivering to customer in Bengal. High quality and nice price refractory fire bricks and thermal insulation materials in Topower Refractory.
As a high temperature refractory industry, the quality of the masonry of the kiln should be quite concerned. The editor of Topower Refractory will explain the use of the following four common refractory fire bricks.
1. Fireclay refractory bricks are an acidic refractory brick, which has good resistance to the parts with acidic slag or gas erosion. Used for fire -resistant masonry for general furnace. Line material. The use temperature of the furnace wall, the bottom of the furnace, the flue, etc. is below 1250 ° C. Burning furnace area, allowing above 1400 ° C
2. High alumina bricks are aluminum silicate -based refractory bricks with high refractory temperature and wear resistance. It is used in general kiln -resistant high temperature resistance and wear -resistant areas or large loads. Required masonry. The vault of the high temperature area of the combustion room allows the use temperature of 1300 ~ 1650 ° C.
3. Lightweight fireclay bricks, also known as insulation insulation clay bricks, are a kind of insulation material. As a furnace -lining for high temperature slag and erosion gas erosion. Essence
4. Lightweight high alumina bricks are also known as high aluminum polymerized light bricks or high aluminum insulation warming bricks. It is used in the heat -resistant lining with a working temperature of less than 1350 ° C , also can directly contact the flame.