In November. 210 tons magnesia chrome bricks are packed for delivering to customer in Belarus. High quality magnesia chrome brick in Topower Refractory.

The production process of firing magnesia chrome brick is similar to that of magnesium bricks. In order to eliminate the loosening effect caused by the expansion of spinels when the bricks reacting the oxide reaction of magnesium, chromium, aluminum or directly combined with magnesia chrome brick iron, it can also be used to make magnesium chromium with synthetic joint feasts to make magnesia chrome brick. There is also no magnesia chrome brick, for example, non -burning magnesium chromium bricks combined with inorganic magnesium salt solution. The production of magnesium chrome brick is simple, low in cost, and good thermal stability, but high temperature intensity is far less than burning bricks. At the end of the 1950s, a direct combination of magnesia chrome brick developed. The characteristics of this kind of brick are pure raw materials, high -temperature firing temperature, directly combined between high -temperature phases such as square magnesium and spinelite, and low melting phase such as siliconate is an island -shaped distribution. Power and slag resistance.

Magnesia chrome brick made of chromium -magnesium ore -magnesium ore powder, magnesia chrome bricks made of high temperature crickets, and high -temperature strength are better than other magnesium chrome bricks. The fine powder made from chromium ore -magnesium sand grinding pressure billets, and the method of combining brick -making with magnesium coarse particles is an effective measure to eliminate the loosening effect. Compared with ordinary types of magnesia chrome brick made of magnesium chrome bricks made of this method, the pores of the bricks are low, and the pressure resistance, load softening temperature, and folding strength are high.
In addition, the molten magnesium chromium with electric furnaces is directly cast magnesia chrome brick, as well as melting particles produced by electric melting magnesium chromium according to the brick -making process.

There are more than 20 R & D teams in Topower Refractory, all of which have many years of production experience in fire resistance materials. They regard quality guarantee and technological innovation as the core competitiveness of the enterprise. In terms of production and management, not only meet customer standards Demand surpassing customers’ expectations.